The reaction kinetics of {311} defect dissolution in SIMOX, SOITEC and bulk silicon materials have been investigated. The effects of implant energy and surface silicon thickness on the activation energy for {311} dissolution have been measured using quantitative TEM (QTEM). SOI wafers having surface silicon thickness of 750 and 1450Å were implanted with Si+ ions at 15-48.5keV, 1 × 1014cm-2. Furnace and RTA anneals were performed at temperatures ranging from 700 to 825 °C. Quantitative TEM was used to monitor the trapped interstitial dose in {311} defects. The activation energy for {311} dissolution was found to decrease as the surface silicon thickness decreased, suggesting a lower activation barrier as the implant damage approaches the surface silicon/buried oxide (BOX) interface. However, the 1450 Å SOI had similar dissolution kinetics to the bulk silicon for all of the implants studied suggesting the reduced activation barrier is likely due to recombination at the surface Si/BOX interface.
Fernando Marianno, Wang Zhou, et al.
INFORMS 2021
Frank R. Libsch, Takatoshi Tsujimura
Active Matrix Liquid Crystal Displays Technology and Applications 1997
S.F. Fan, W.B. Yun, et al.
Proceedings of SPIE 1989
O.F. Schirmer, W. Berlinger, et al.
Solid State Communications