S. Cohen, J.C. Liu, et al.
MRS Spring Meeting 1999
The progressive reduction of SrTiO3 has been monitored by EPR. The results show the conversion of Mn4+ to Mn2+ and Mn2+ to Mn2+-V0 by oxygen-vacancy capture. The latter defect association takes place with the copious oxygen vacancies produced during high-temperature reduction between 1100 - 1300 K. At still higher reduction temperatures, other defects are formed. Analysis of the temperature dependence of the defect association gives a value of 0.7 eV for the enthalpy of association. © 1983.
S. Cohen, J.C. Liu, et al.
MRS Spring Meeting 1999
I.K. Pour, D.J. Krajnovich, et al.
SPIE Optical Materials for High Average Power Lasers 1992
A. Nagarajan, S. Mukherjee, et al.
Journal of Applied Mechanics, Transactions ASME
A. Gangulee, F.M. D'Heurle
Thin Solid Films