CoWP metal caps for reliable 32 nm 1X Cu interconnects in porous ULK (k=2.4)E. HuangM. Ohet al.2009ADMETA 2009
UV curing-induced photoresist poisoning in advanced ULK BEOL integration schemesY.C. EeD. Kioussiset al.2009ADMETA 2009
Comparison of electromigration in Cu interconnects with ALD or PVD TaN linersC.-K. HuL. Gignacet al.2006ECS Meeting 2006
65nm Cu integration and interconnect reliability in low stress K=2.75 SiCOHV. McGahayG. Bonillaet al.2006IITC 2006
Post copper CMP hybrid clean process for advanced BEOL technologyWei-Tsu TsengVamsi Devarapalliet al.2013IEEE Trans Semicond Manuf
Comparison of electromigration in Cu interconnects with atomic-layer- or physical-vapor-deposited TaN linersC.-K. HuL. Gignacet al.2007JES