P.C. Pattnaik, D.M. Newns
Physical Review B
The rate of silicon etching by XeF2 is dependent on the type of dopant and the doping level. Soft-x-ray photoemission was used in an effort to elucidate the mechanism responsible for this phenomenon. Si(111) samples were subjected to sufficient XeF2 to reach the steady-state etching regime, and spectra were collected of the fluorosilyl reaction intermediate species that form on the surface. Samples that were lightly doped (1017 cm-3) showed virtually no difference between p and n doping, while heavily doped samples (1020 cm-3) showed a marked difference. The heavily doped n-type sample had a slightly thinner reaction layer than did the lightly doped samples, while the heavily doped p-type sample had a much thicker layer, in which the composition of the layer was also changed. These results are discussed in terms of possible reaction mechanisms. © 1988 The American Physical Society.
P.C. Pattnaik, D.M. Newns
Physical Review B
Dipanjan Gope, Albert E. Ruehli, et al.
IEEE T-MTT
Frank R. Libsch, Takatoshi Tsujimura
Active Matrix Liquid Crystal Displays Technology and Applications 1997
Heinz Schmid, Hans Biebuyck, et al.
Journal of Vacuum Science and Technology B: Microelectronics and Nanometer Structures